RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of CDGM - QF (Light flint)
QF5

Wavelength: µm
 (0.365 – 0.7065)  
 

Other optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.4440594-6.7974631\text{×}10^{-3}λ^{2}+2.1425387\text{×}10^{-2}λ^{-2}-3.8544649\text{×}10^{-4}λ^{-4}+1.2195244\text{×}10^{-4}λ^{-6}-4.2162236\text{×}10^{-6}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

CDGM Optical Glass Products Database