Optical constants of CDGM - F (Flint)
H-F51

Wavelength: µm
 (0.365 – 0.7065)  
 

Other optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.6334392-2.3786997\text{×}10^{-2}λ^{2}+1.3503973\text{×}10^{-2}λ^{-2}+3.9049789\text{×}10^{-3}λ^{-4}-4.141067\text{×}10^{-4}λ^{-6}+2.7097419\text{×}10^{-5}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

CDGM Optical Glass Products Database