Optical constants of CDGM - F (Flint)
F1

Wavelength: µm
 (0.365 – 0.7065)  
 

Other optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.5059651-7.8686119\text{×}10^{-3}λ^{2}+2.1574214\text{×}10^{-2}λ^{-2}+5.9867966\text{×}10^{-4}λ^{-4}-9.5194606\text{×}10^{-7}λ^{-6}+2.9024858\text{×}10^{-6}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers