Optical constants of CDGM - BAF (Barium flint)
BAF4

Wavelength: µm
 (0.365 – 0.7065)  
 

Other optical constants

logX   logY   eV

Dispersion formula

$$n^2=2.451472-6.5118879\text{×}10^{-3}λ^{2}+1.9377342\text{×}10^{-2}λ^{-2}-3.0637647\text{×}10^{-4}λ^{-4}+1.0174985\text{×}10^{-4}λ^{-6}-3.9270356\text{×}10^{-6}λ^{-8}$$

Comments

Refractive index is relative to air at standard conditions; Wavelength in dispersion formula is as measured in air and expressed in micrometers

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

CDGM Optical Glass Products Database

More info - wiki

-