Optical constants of BARBERINI - Sun Protection
D9148: Rosalite 9148 UV

Wavelength: µm
 (0.43583 – 0.65627)  
 

Other optical constants

logX   logY   eV

Comments

20 °C
Sun Protection Glass; Colour: dark rose; Application: light tinted sunglare filter with contrast intensification red / yellow and high UV - absorption filter category 1 acc. to DIN EN 1836

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

Barberini D9148 glass specifications, 2010-08

More info - wiki

Barberini GmbH is a German branch of Barberini S.p.A., the Italian company specializing in ophthalmic materials. Barberini GmbH has been formed after Barberini acquired the ophthalmic division of Schott AG in 2010.