Optical constants of BARBERINI - Moulds
D0191: CH-5555

Wavelength: µm
 (0.43583 – 0.65627)  
 

Other optical constants

logX   logY   eV

Comments

20 °C
Mold Glass; Colour: clear; Application: Special glass, in particular suitable for a rapid chemical toughening without problems. The ideal material for moulds for the manufacture of plastic lenses.

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

Barberini D0191 glass specifications, 2010-06

More info - wiki

Barberini GmbH is a German branch of Barberini S.p.A., the Italian company specializing in ophthalmic materials. Barberini GmbH has been formed after Barberini acquired the ophthalmic division of Schott AG in 2010.