RefractiveIndex.INFO Refractive index database

Shelf

Book

Page

Optical constants of BARBERINI - High Index
D0082: LaSF 1.9/30

Wavelength: µm
 (0.43583 – 0.65627)  
 

Other optical constants

logX   logY   eV

Comments

20 °C
High Index Glass; Colour: clear; Application: High index light weight glass for corrective lenses with very high power

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

Barberini D0082 glass specifications, 2010-08

More info - wiki

Barberini GmbH is a German branch of Barberini S.p.A., the Italian company specializing in ophthalmic materials. Barberini GmbH has been formed after Barberini acquired the ophthalmic division of Schott AG in 2010.