Optical constants of BARBERINI - Normal Crown
D0290: HC-Weiss 0290

Wavelength: µm
 (0.43583 – 0.65627)  
 

Other optical constants

logX   logY   eV

Comments

20 °C
Normal Crown Glass (Uni/Bifocal); Colour: clear; Application: High index glass for corrective lenses

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

References

Barberini D0290 glass specifications, 2010-06

More info - wiki

Barberini GmbH is a German branch of Barberini S.p.A., the Italian company specializing in ophthalmic materials. Barberini GmbH has been formed after Barberini acquired the ophthalmic division of Schott AG in 2010.