Optical constants of Titanium (Ti)

From RefrectiveIndex.INFO - Refractive index database

Optical constants of Titanium (Ti)
Wavelength: µm  (0.2066~1.24)
Refractive index (real part of complex index of refraction)

Refractive index - Wikipedia

n = 3.62

Chromatic dispersion

Dispersion (optics) - Wikipedia

dn/dλ = 1.314 µm-1

[ Figure: Refractive index of Titanium (Ti) ]
Extinction coefficient (imaginary part of complex index of refraction)

Dispersion and absorption - Wikipedia

k = 3.5200e+0

Absorption coefficient

Attenuation coefficient - Wikipedia

α = 3.5672e+5 cm-1

[ Figure: Extinction coefficient of Titanium (Ti) ]
Tabulated data (n, k)

csv (comma separated)   txt (tab separated)

References

SOPRA N&K Database [link]

Optical transmission calculator
Thickness : 
Include reflection (normal incidence, two surfaces)
Transmittance (at 1.24 µm)

Transmittance - Wikipedia

T = ...

Reflection calculator
Angle of incidence (0~90°): 
Direction: in out
Reflectance (at 1.24 µm)

Fresnel equations - Wikipedia

RS = ... (S-polarized)
RP = ... (P-polarized)
R = ... (non-polarized, (RS+RP)/2 )

Reflection phase

ɸ = ...°
ɸS = ...°
ɸP = ...°

Brewster's angle

Brewster's angle - Wikipedia

θB = ...°

Critical angle

Total internal reflection - Wikipedia

θC = ...°

More info ( wiki ) [ edit ]