RefractiveIndex.INFO

Refractive index database

Database   Wiki   Forum

Optical constants of Heavy water (D₂O)

From RefrectiveIndex.INFO - Refractive index database

Optical constants of Heavy water (D2O)
Wavelength: µm  (0.40466~0.7682)
Refractive index

Refractive index - Wikipedia

n = 1.32848

Chromatic dispersion

Dispersion (optics) - Wikipedia

dn/dλ = -0.0269 µm-1

Abbe numbers

Abbe number - Wikipedia

Vd = 61.06

Ve = 60.95

Formulae    Abbe diagram

[ Figure: Refractive index of Heavy water (D2O) ]
Tabulated data

csv (comma separated)   txt (tab separated)

Conditions

T = 293 K; P = 0.101325 MPa

References

- Properties of Optical and Laser-Related Materials: A Handbook, D. N. Nikogosyan. John Willey Sons 1997 [link]

Reflection calculator
Angle of incidence (0~90°): 
Direction: in out
Reflectance (at 0.58756 µm)

Fresnel equations - Wikipedia

RS = ... (S-polarized)
RP = ... (P-polarized)
R = ... (non-polarized, (RS+RP)/2 )

Reflection phase

ɸ = ...°
ɸS = ...°
ɸP = ...°

Brewster's angle

Brewster's angle - Wikipedia

θB = ...°

Critical angle

Total internal reflection - Wikipedia

θC = ...°

More info ( wiki ) [ edit ]

Heavy water, D2O

Other names: Water-d2, Dideuterium monoxide

Contents

Optical properties

--- add info ---

Other properties

--- add info ---

Refractive index database entry

External links

References

© 2008-2012 Mikhail Polyanskiy   |   Link to or cite RefractiveIndex.INFO   |   NO GUARANTEE OF ACCURACY - Use on your own risk