n = 1.46991 Chromatic dispersion
dn/dλ = -0.0305 µm-1 |
|
25 °C
- J. Rheims, J. Köser and T. Wriedt. Refractive-index measurements in the near-IR using an Abbe refractometer, Meas. Sci. Technol. 8, 601-605 (1997) doi:10.1088/0957-0233/8/6/003
|