Carbon, C
Most common allotropes
Diamond (cubic carbon); Graphite; Amorphous carbon
From RefrectiveIndex.INFO - Refractive index database
|
n = 2.41748 Chromatic dispersion
dn/dλ = -0.131 µm-1 Abbe numbers
Vd = 55.30 Ve = 54.86 |
|
Room temperature
- Handbook of Optics, 3rd edition, Vol. 4. McGraw-Hill 2009 [link]
- Other name: Cubic carbon
|
Reflectance (at 0.5876 µm)
RS = ... (S-polarized) Reflection phase
ɸ = ...° Brewster's angle
θB = ...° Critical angle
θC = ...° |
Carbon, C